Combined Strengthening of Batan Teeth of the Stb Loom
Abstract
The combined strengthening of the batan teeth of the STB loom is considered, including chemical and thermal treatment-nitrocementation and surface plastic deformation in the form of shot blasting. Shot hardening forms compressive residual stresses in the surface layer, which, together with the increased hardness, increases the wear resistance of the batan teeth.
References
Khudykh M. I. Repair of textile machines.- M: Legprombytizdat, 1991. - 288 p.
Papshev D. D. Finishing and strengthening treatment with surface plastic deformation-Moscow: Mashinostroenie, 1978 – - 152 p.
Suslov A. G. Quality of the surface layer of machine parts. - M.: Mashinostroenie, 2000. - 320 p.
Tehnologiyatekstilnogomashinostroeniya / ed. by L. K. Sizenova-M.: Mashinostroenie, 1988. - 320 p.
Pirogov K. M., Vyatkin B. A. Fundamentals of reliability of textile machines. - M: Legprombytizdat, 1985. - 256 p.
Balter M. A. Strengthening of machine parts – - M.: Mashinostroenie, 1978 – - 184 p.
Shin .I. G., Maksudov R. Kh. Method for calculating the depth of the hardened layer of parts during surface treatment with shot // Bulletin of Mechanical Engineering. - Moscow, 2011, No. 4. - p. 44-47.